MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyrocks Chemical EP8400S90F-H3 Polyolefin Cable Compound
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: EP8400S90F-H3 is thermoplastic low smoke halogen free polyolefin cable compound, which formed by mixing, milling and granulating of polyolefin resin combined environmental inorganic flame retardant additives and other additives, having excellent Mechanical properties, electrical properties, flame retardant performance and processing performance. Burning without halogen acid gas, releasing very few toxicity and corrosive gas, with low smoke, etc.

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccASTM D792
pH >= 5.0IEC 60754-2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 53ASTM D2240
Tensile Strength 13.0 MPaIEC 60811-1-1
 13.5 MPa
@Temperature 100 °C,
Time 245000 sec
Aging; IEC 60811-1-2
Elongation at Break 201 %IEC 60811-1-1
 197 %
@Temperature 100 °C,
Time 245000 sec
Aging; IEC 60811-1-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.10e+14 ohm-cmIEC 60093
 1.50e+14 ohm-cm
@Temperature 70.0 °C,
Time 605000 sec
Immersion; IEC 60093
Dielectric Strength 34.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -25.0 °CPass; IEC 60811-1-4
Smoke Density 76Flaming; ASTM E-662
 237Non-Flaming; ASTM E-662
Oxygen Index 33 %ASTM D2863
 
Descriptive Properties
Electrical conductivity<2 µS/mmIEC 60754-2
Halogen acid gas0 mg/gIEC 60754-1
Heat Shrinkage0.011100°C × 1h, IEC60811-13
High Temperature Pressure0.3380°C×4h, IEC 60811-3-1
Toxicity1NES 713-1985

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROCKS024 / 278532

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.