MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Wacker Silpuran® 6700/60 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product description: Liquid silicone rubber of the SILPURAN® 6700 series is a paste-like, easily-pigmentable two-component compound with a very short curing time and good mechanical and electrical properties. Vulcanizates are noted for their self-adhesive properties to various substrates.

Properties: SILPURAN® 6700/60 A/B meets selected test requirements of ISO 10993 and United States Pharmacopoeia (USP) Class VI. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Special features: SILPURAN® 6700/60 A/B is a primerless selfbonding grade that adheres to various thermoplasts (e.g. PA, PBT) and metals. The bonding is improved by an ageing process (e.g. one hour at 100 °C) or by a longer storage at room temperature. Because of the individual surface properties each substrate must be tested before mass production. If necessary one has to check the development of adhesive properties over time and/or in an environment relevant to the application.

Application: SILPURAN® 6700/60 A/B is particularly suitable for the economical production of large series of injection-moulded articles. SILPURAN® 6700/60 A/B is designed for medical and pharmaceutical applications including implantation for < 30 days.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccDIN EN ISO 1183-1 A
Viscosity 500000 cP
@Shear Rate 10.0 1/s
DIN 53019
 1.70e+6 cP
@Shear Rate 1.00 1/s
DIN 53019
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60DIN 53505
Tensile Strength at Break 8.20 MPaDIN 53505 S1
Elongation at Break 490 %DIN 53505 S1
Rebound 60 %DIN 53512
Tear Strength 28.0 kN/mASTM D624B
Compression Set 60 %
@Temperature 125 °C,
Time 79200 sec
DIN ISO 815-B
 70 %
@Temperature 150 °C,
Time 79200 sec
DIN ISO 815-B
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Colortransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3842/60 A/B Liquid Silicone Rubber
Wacker Silpuran® 8060/60 Silicone Rubber
Wacker Silpuran® 8461/60 Silicone Rubber
Wacker Elastosil® R 420/70 Silicone Rubber
Wacker ELASTOSIL® R 407/60 Silicone Rubber Base

PWACK9505 / 205034

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.