MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ConocoPhillips Hydroclear Diamond Class® AW Turbine Oil 32
Categories: Fluid; Lubricant

Material Notes: Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe service. Diamond Class AW Turbine Oil is formulated with premium hydrocracked base oils and select additives to provide outstanding oxidation resistance, excellent wear protection, protection against rust and corrosion, and resistance to foaming. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It protects system components against rust and corrosion. It has excellent water-separating properties to minimize the formation of emulsions and is resistant to excessive foam buildup that can interfere with proper lubrication. An ashless (non-zinc) antiwear additive provides wear protection for gears and bearings. Diamond Class AW Turbine Oil is filtered to an ISO Cleanliness Code of 18/16/13 for use in circulating systems with tight tolerances where particle contamination can cause operational problems. The bulk oil is filtered at the blending terminal prior to filling any package containers, and is filtered again upon delivery in bulk to the customer’s bulk tank.

Applications:

  • Combined-cycle and co-generation gas turbines
  • Gas turbines and steam turbines with gear drives
Diamond Class AW Turbine Oil meets the requirements of the following industry and OEM specifications:
  • ABB G12106
  • Alstom Power HTGD 90 117, for turbines with gear drives
  • ASTM D4304-06a, Type II Turbine Oil
  • British Standard 489
  • DIN 51515 Part 1, Lubricating Oils, Type L-TD
  • DIN 51515 Part 2, Lubricating Oils, Type L-TG
  • DIN 51517 Part 1, Lubricating Oils, Type CL
  • DIN 51524 Part 1, Hydraulic Oils, Type HL DIN 51524 Part 2, Antiwear Hydraulic Oils, Type HLP
  • Elliott ring-oiled turbines, where mineral-based turbine oil is Specified
  • General Electric GEK 101941A, GEK 107395A, GEK 32568F, GEK 46506e, GEK 27070 (obsolete), GEK 28143A (obsolete)
  • Siemens Power Generation TLV 9013 04, TLV 9013 05
  • Siemens Westinghouse 21T0591 (obsolete), 55125Z3 (obsolete)
  • Solar Turbines ES9-224, Rev. W, Class II Turbine Oil
  • U.S. Military MIL-PRF-17672D, Symbol 2075 T-H (ISO VG 32), 2110 T-H (ISO VG 46), 2135 T-H (ISO VG 68)
  • U.S. Steel 126
Features/Benefit:
  • Outstanding oxidation resistance and thermal stability for long service life
  • Protects against sludge and varnish formation
  • Excellent wear protection for gears and bearings
  • Protects against rust and corrosion
  • Excellent water-separating properties
  • Resists the formation of emulsions and bacteria buildup
  • Good foam resistance
  • Meets ISO Cleanliness Code rating of 18/16/13

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.862 g/cc
Density 7.18 lb/gal
Viscosity Measurement 102Viscosity Index
Saybolt Viscosity at 100°F 165 SUS
Saybolt Viscosity at 210°F 44 SUS
Kinematic Viscosity at 40°C (104°F) 32 cSt
Kinematic Viscosity at 100°C (212°F) 5.4 cSt
Oxidative Stability >= 24000 hourTOST, (modified),; ASTM D943-04a
ASTM Color 0.50
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.14[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.500 mmScar Diameter; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -39.0 °F
Rotating Bomb Oxidation Test (RBOT) >= 1700 minASTM D 2272
Flash Point 428 °FCOC
 
Descriptive Properties
Air Release2.2 minsASTM D3427
Corrosion, Copper Strip1AASTM D130
Emulsion Characteristics (40-40-0)10 minutesWater Separation
FZGPass 9 Stages

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Phillips 66 Multipurpose R&O Oil ISO Grade 32
ExxonMobil 32 Mobil Mist Lube Series
ExxonMobil 24 Mobil Mist Lube Series

WCON075 / 75112

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.