MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celanex® 2002-3 PBT, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains an internal lubricant.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Moisture Absorption 0.250 %23°C/50%RH; ISO 62
Viscosity Test 140 cm³/gISO 307, 1157, 1628
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
[cm3/10min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPa50mm/min; ISO 527-2/1A
Elongation at Break >= 50 %
Elongation at Yield 4.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 2500 MPa50mm/min; ISO 527-2/1A
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 2500 MPaISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
Charpy Impact Unnotched NBISO 179/1eU
 190 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°CISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75-1, -2
Vicat Softening Point 190 °CISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 96.0 °Ccavity
 250 - 260 °Chot runner
Feed Temperature 230 - 240 °C
Zone 1 230 - 240 °C
Zone 2 235 - 250 °C
Zone 3 235 - 250 °C
Zone 4 240 - 260 °C
Die Temperature 240 - 260 °C
Melt Temperature 235 - 260 °C
 250 °CISO 294
Mold Temperature 80.0 °CISO 294
Injection Velocity 250 mm/secISO 294
Drying Temperature 120 - 130 °C
Dry Time 4.00 hour
Moisture Content <= 0.020 %
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 1602Z PBT, Unfilled
Celanese Celanex® 1700FC PBT, Unfilled
Celanese Celanex® 2000-3 PBT, Unfilled
Celanese Celanex® 2000-3FC PBT, Unfilled
Celanese Celanex® 2500 PBT, Unfilled

PHCQ018 / 178473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.