Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according to the required surface properties. Availability: Africa & Middle East and Europe Additive: - Antiblock: 1750 ppm
- Slip: No
- Thermal Stabilizer: Yes
Information provided by ExxonMobil |