MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay 70000 Aramid Peel
Categories: Polymer; Thermoset; Aramid

Material Notes: Description: Peel ply. Ideally suited to aerospace applications.

Features & Benefits:

  • Aramid peel ply
  • Designed for high temperature applications
  • Available coated and non-coated, depending on user requirement
  • Imparts a coarse weave pattern when removed from the composite laminate
  • Manufactured by Precision Fabrics Group (PFG)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 427 °C
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Nomex® N102 Texturized Filament Yarn
DuPont™ Nomex® 430 1600 Denier Aramid Yarn
DuPont™ Nomex® N104 Dyeable Filament Yarn
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm

PCYTED259 / 180561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.