MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

General Plastics LAST-A-FOAM® FR-4512 High Density, Rigid Foam
Categories: Other Engineering Material

Material Notes:

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.192 g/cc0.00694 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.90 MPa276 psiPerpendicular to Rise; ASTM D1623
 2.00 MPa290 psiParallel to Rise; ASTM D1623
Flexural Strength 2.83 MPa410 psiRise Parallel to Test Span; ASTM D790 Method 1-A
 2.84 MPa412 psiRise Parallel to Beam Thick.; ASTM D790 Method 1-A
Flexural Modulus 0.12682 GPa18.393 ksiRise Parallel to Beam Thick.; ASTM D790 Method 1-A
 0.12895 GPa18.703 ksiRise Parallel to Test Span; ASTM D790 Method 1-A
Compressive Strength  1.84 MPa
@Temperature 71.1 °C
267 psi
@Temperature 160 °F
Perpendicular to Rise; ASTM D1621
 1.95 MPa
@Temperature 71.1 °C
283 psi
@Temperature 160 °F
Parallel to Rise; ASTM D1621
 2.45 MPa
@Temperature 23.9 °C
356 psi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
 2.49 MPa
@Temperature 23.9 °C
361 psi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
Compressive Modulus  0.069272 GPa
@Temperature 71.1 °C
10.047 ksi
@Temperature 160 °F
Parallel to Rise; ASTM D1621
 0.069306 GPa
@Temperature 71.1 °C
10.052 ksi
@Temperature 160 °F
Perpendicular to Rise; ASTM D1621
 0.079028 GPa
@Temperature 23.9 °C
11.462 ksi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 0.080689 GPa
@Temperature 23.9 °C
11.703 ksi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
Poissons Ratio 0.300.30
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.2 µm/m-°C
@Temperature -45.6 - 93.3 °C
29.0 µin/in-°F
@Temperature -50.0 - 200 °F
GP Method
Thermal Conductivity 0.0425 W/m-K0.295 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 103 °C217 °FASTM E1824
 
Descriptive Properties
Surface Roughness1131sanded, SJ-201P per JIS B0601-1982
Tumbling Friability (%)2.5220 mins at 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGENR023 / 186809

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.