ALKROTHAL 3 is a ferritic FeCrAl alloy which is recommended for use at temperatures up to 1000°C (1830°F). Typical applications for ALKROTHAL 3 are in rheostats, braking resistors, etc. It is also used as electrical heating elements in industrial applications. Information provided by Sandvik |