MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Halsic I (reaction-bonded, silicon infiltrated) Silicon Carbide
Categories: Ceramic; Carbide

Material Notes: Exceptionally high-performance ceramics, offering absolute dimensional stability under high loads at elevated temperatures. Extremely high corrosion resistance. Very good thermal shock resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.70 - 3.10 g/cc0.0975 - 0.112 lb/in³Fired
Porosity 0.10 - 5.0 %0.10 - 5.0 %Apparent, water absorption
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 420 GPa60900 ksidynamic
 280 - 370 GPa
@Temperature 20.0 °C
40600 - 53700 ksi
@Temperature 68.0 °F
Flexural Strength 80.0 - 400 MPa
@Temperature 20.0 °C
11600 - 58000 psi
@Temperature 68.0 °F
3-point
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.30 - 5.00 µm/m-°C
@Temperature 20.0 - 1000 °C
2.39 - 2.78 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 35.0 - 124 W/m-K
@Temperature 200 °C
243 - 861 BTU-in/hr-ft²-°F
@Temperature 392 °F
Maximum Service Temperature, Air 1300 - 1650 °C2370 - 3000 °Fworking

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Silicon Carbide, Reaction-Bonded, SiSiC
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Anderman Ceramics EC100P Recrystallized Silicon Carbide
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%)

CMORG57 / 90435

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.