Zeoforte® ZSC 2295CX is a highly saturated copolymer of butadiene and acrylonitrile which has been modified with the zinc salt ofmethacrylic acid utilizing an advancedmicro-mixture technology. ZSC 2295CX has excellent physical properties and abrasion resistance over a wide variation of temperatures. Highly saturated copolymer of butadiene and acrylonitrile which has been modified with the zinc salt of methacrylic acid utilizing an advanced micro-mixture technology. ZSC 2295CX has excellent physical properties and abrasion resistance over a wide variation of temperatures. |