MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ChevronTexaco FM Trolley Oil
Categories: Fluid; Lubricant

Material Notes: Chevron Trolley Oil FM is a tasteless, odorless, high viscosity index paraffinic lubricating oil combined with additives that provide lubricity and rust protection, antiwear performance, and tackiness to minimize oil drippings.

This product provides performance well above that found in typical white mineral oils often used in the food industry.

Applications

Chevron Trolley Oil FM is designed for the lubrication and rust prevention of trolley hooks and bearings in meat processing plants.

This lubricant emulsifies readily with caustic solutions to form a detergent that helps to clean animal fat from the trolley hooks.

Chevron Trolley Oil FM contains lubricity agents that promote free movement of the trolleys without sticking.

Key Words: CPS Number: 266161; MSDS Number: 6176
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32.2 °
Viscosity Measurement 120ASTM D2270
Saybolt Viscosity at 100°F 226 SUS
Saybolt Viscosity at 210°F 49.9 SUS
Kinematic Viscosity at 40°C (104°F) 44 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.1 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -14.0 °CASTM D97
Flash Point 226 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco FM ISO 460 Lubricating Oil
ChevronTexaco Amber Petrolatum
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded

WCHEV113 / 74728

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.