MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, Viscoelastic
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Information provided by Bayer Corporation, Polyurethanes Division

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0480 g/ccASTM D3574A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 0.130 MPaASTM D3574E
Elongation at Break 176 %ASTM D3574E
Tear Strength 0.540 kN/mDie C; ASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, High-Resilience
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)

PB2B63 / 26610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.