MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF 2,5-Dimethyl-2,5-hexanediol
Categories: Fluid

Material Notes: Formula: C8H18O2

CAS: 110-03-2

Description: Dimethylhexanediol is a colorless to yellow solid, and is odorless. It is soluble in water and easily soluble in alcohols and acetone.

Synonyms: 2,5-Dimethylhexanediol-2,5

Applications: Intermediate used in the production of Pesticides, Plastics processing industry and Organic peroxide

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 g/cc
Molecular Weight 146.2 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 87.0 - 90.0 °C
Boiling Point 214 - 215 °C
Flash Point >= 104 °C
Ignition Temperature 420 °C
 
Descriptive Properties
Assay>99.5%
Color<20APHA, DIN EN 1557
Iodine number<1 g Iodine/100g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Esstech X-690-0000 1,9-Nonanediol Diacrylate, C15H24O4
BASF HDO® 1,6-Hexanediol Molten
BASF 1,6-Dichlorohexane
3,4-Dichlorobenzotrifluoride, C7H3Cl2F3

PBASG0916 / 132549

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.