System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Dow VORANOL™ CP 4702 Polyol
Categories:
Polymer
;
Thermoset
Material Notes:
VORANOL™ CP 4702 polyol is a high reactivity, capped triol, polyether polyol especially designed for the production of molded flexible foam. It is normally used in all TDI or TDI/MDI blend formulations.
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.026
g/cc
pH
7.0 - 9.0
(1 Water / 10 Methanol); DOWM 101495-TE94A
Viscosity Measure
434
cSt
@Temperature 37.8 °C
ASTM D445-94
750
-
870
cSt
@Temperature 25.0 °C
ASTM D445-94
Molecular Weight
4700
g/mol
Maximum Moisture Content
0.060
wt% water; ASTM E203-96
ASTM Color
<= 30
APHA; ASTM D4890-93
Chemical Properties
Original Value
Comments
Total Acid Number
0.050
[mg KOH/g]; DOWM 100387-TE95A
Thermal Properties
Original Value
Comments
Flash Point
248
°C
C.O.C.
Descriptive Properties
Hydroxyl Number mg KOH/g
33.7 - 37.3
ASTM D4274-94d
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Dow VORANOL™ 4701 Polyether Polyol
Dow VORANOL™ 4815 Polyether Polyol
Dow VORANOL™ 4703 Polyether Polyol
Dow VORANOL™ 4240 Polyether Polyol
Dow SPECFLEX™ NC 700 Polyol
PDOW1478 / 30696
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.