Trigonox 23-C75 is an initiator (75% active ingredient in odorless mineral spirits) for (co)polymerization of (meth)acrylates. CAS number: 26748-41-4 EINECS/ELINCS No: 247-955-1 Applications: Polymerization of ethylene: Trigonox 23-C75 is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range. Trigonox 23-C75 is a highly reactive initiator for curing unsaturated polyester and vinyl ester resins at elevated temperatures. It is typically used in combination with higher temperature finishing initiators in pultrusion and continuous panel applications. Information provided by Nouryon |