MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CLAL-MSX CUPROROR® TL1 1/4 hard, Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperature stability. CUPROFOR® is used in the manufacture of high power transistor supports, integrated circuits, electrical contacts and shunts.

Applications:

Electronics

Heat sinks for power transistors

CUPROFOR® properties include

  • Thermal conductivity to dissipate heat
  • Temperature resistance permitting Pb/Sn soldering of the chip without loss of mechanical properties
  • Mechanical strength to prevent deformation of heat dissipaters when moulding. CUPROFOR® can play an important part in the manufacture of power transistor heat sinks.

For this application, CLAL offer 1/2 hard profile strips (condition TL2) in long length coils which can be delivered :

  • totally or partially Ni coated, with an inlay of Pb/Sn, Ag or other material.

Support media for printed circuits

This application uses the following properties :

  • temperature resistance, thus permitting the soldering of the integrated circuit of the DIE PAD, without loss of hardness in the support media
  • Outstanding mechanical properties which guarantees the mechanical strength of the LEADS
  • A high deformation capacity gives suitability to form external LEADS.
For this application, CLAL, upon request offer long length tapes :
  • a high standard of geometrical and dimensional accuracy
  • a stress relieving treatment to maintain that the LEADS TIPS are coplanar about the DIE PAD.

The electro-technical field

  • Electrical contacts
  • Contact mounts
  • Pushbuttons
  • Conductive parts
  • Electrical connections and terminals.
Other fields
  • Heat exchangers
  • Seals and washers
  • Dephasing rings.

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 100 - 125100 - 125
 108
@Temperature 500 °C,
Time 180 sec
108
@Temperature 932 °F,
Time 0.0500 hour
Isotherm
 108
@Temperature 500 °C,
Time 600 sec
108
@Temperature 932 °F,
Time 0.167 hour
Isotherm
 108
@Temperature 500 °C,
Time 1800 sec
108
@Temperature 932 °F,
Time 0.500 hour
Isotherm
 109
@Temperature 500 °C,
Time 60.0 sec
109
@Temperature 932 °F,
Time 0.0167 hour
Isotherm
 109.5
@Temperature 350 °C,
Time 1800 sec
109.5
@Temperature 662 °F,
Time 0.500 hour
Isotherm
 110
@Temperature 350 °C,
Time 180 sec
110
@Temperature 662 °F,
Time 0.0500 hour
Isotherm
 110
@Temperature 350 °C,
Time 600 sec
110
@Temperature 662 °F,
Time 0.167 hour
Isotherm
 110
@Temperature 500 °C,
Time 30.0 sec
110
@Temperature 932 °F,
Time 0.00833 hour
Isotherm
 110.5
@Temperature 500 °C,
Time 10.0 sec
110.5
@Temperature 932 °F,
Time 0.00278 hour
Isotherm
 110.5
@Temperature 350 °C,
Time 60.0 sec
110.5
@Temperature 662 °F,
Time 0.0167 hour
Isotherm
 111
@Temperature 350 °C,
Time 30.0 sec
111
@Temperature 662 °F,
Time 0.00833 hour
Isotherm
 111
@Temperature 500 °C,
Time 0.000 sec
111
@Temperature 932 °F,
Time 0.000 hour
Isotherm
 112
@Temperature 350 °C,
Time 0.000 sec
112
@Temperature 662 °F,
Time 0.000 hour
Isotherm
 112
@Temperature 350 °C,
Time 10.0 sec
112
@Temperature 662 °F,
Time 0.00278 hour
Isotherm
Tensile Strength, Ultimate 320 - 400 MPa46400 - 58000 psi
Tensile Strength, Yield >= 220 MPa
@Strain 0.2 %
>= 31900 psi
@Strain 0.2 %
Elongation at Break >= 15 %>= 15 %LO=5.65vSO
Modulus of Elasticity 140 GPa20300 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000181 - 0.00000229 ohm-cm0.00000181 - 0.00000229 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.3 µm/m-°C
@Temperature 0.000 - 500 °C
9.06 µin/in-°F
@Temperature 32.0 - 932 °F
 16.4 µm/m-°C
@Temperature 0.000 - 250 °C
9.11 µin/in-°F
@Temperature 32.0 - 482 °F
 16.7 µm/m-°C
@Temperature 0.000 - 100 °C
9.28 µin/in-°F
@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.383 J/g-°C0.0915 BTU/lb-°F
Thermal Conductivity 338 W/m-K2350 BTU-in/hr-ft²-°F
Melting Point 1080 °C1980 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 0.080 %0.080 %
Copper, Cu 99.84 %99.84 %As Balance
Phosphorus, P 0.080 %0.080 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
17-7 PH Stainless Steel, CH900, plate, sheet, and strip
Beryllium, Be
Copper, UNS C70400
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO50 Temper flat products
CLAL-MSX CUPROROR® TL4 Hard, Copper Alloy

NCLAL036 / 160067

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.