Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected. Suitable as high-frequency insulation on account of the low dielectric loss factor.Information provided by Elektro-Isola |
IEC/EN 60893-3-1 PF CP 206, DIN 7735 Hp 2062.8, NF C26 150 PPP0, BS 2572 P3/1, NEMA LI 1 XXX |