MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M AC-736 B-2 Aerospace Sealant
Categories: Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: 3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an effective barrier against the common causes of corrosion on aluminum and between dissimilar metals. 3M AC-736 B-2 Sealants has outstanding resistance to aviation gasoline and jet fuel, as well as resistance to chemicals, hydraulic fluids and petroleum products common to the aircraft industry. 3M AC-736 B-2 Sealant maintains its flexibility and bond strength on most metal substrates such as aluminum, titanium, steel, stainless steel, and many other extremes for temperature, weathering and stress. The mixed compound is a flowable, fay surface grade material, easily applied by spatula, brush, roller or extrusion gun. They maintain flexibility and bond strength on most metal substrates under extremes of temperature, weathering stress.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³cured 14 days @ 50% RH
Volatiles 4.0 %4.0 %
Brookfield Viscosity 900000 - 1.60e+6 cP900000 - 1.60e+6 cPBase, RVF #7 sp @ 2 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 42 - 4842 - 48cured 14 days @ 50% RH
Tensile Strength at Break 1.59 MPa
@Temperature 336 °C
231 psi
@Temperature 637 °F
MIL-PRF-81733 AND AS5127A
 1.86 MPa
@Thickness 3070 mm,
Temperature 168 °C
270 psi
@Thickness 121 in,
Temperature 334 °F
MIL-PRF-81733 AND AS5127A
 1.86 MPa
@Treatment Temp. 121 °C,
Time 605000 sec
270 psi
@Treatment Temp. 250 °F,
Time 168 hour
MIL-PRF-81733 AND AS5127A
Elongation at Break 170 %170 %72 hrs in JRF is 60°C, 72 hrs at 49°C, 7 days at 121°C; MIL-PRF-81733 AND AS5127A
 390 %
@Time 1.21e+6 sec
390 %
@Time 336 hour
Standard Cure; MIL-PRF-81733 AND AS5127A
 120 %
@Treatment Temp. 121 °C,
Time 605000 sec
120 %
@Treatment Temp. 250 °F,
Time 168 hour
MIL-PRF-81733 AND AS5127A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °Fcured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °C-65.2 °Fcured 14 days @ 50% RH
 
Processing PropertiesMetricEnglishComments
Cure Time 720 min12.0 hour
Tack-Free Time 720 min12.0 hour
Shelf Life 9.00 Month
@Temperature <=26.7 °C
9.00 Month
@Temperature <=80.1 °F
 
Descriptive Properties
AppearanceBrownAccelerator
 Dark Brown
 Off WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35407 / 170154

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.