MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Radici Radilon® D RV400RG 3900 BK Polyamide 610
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: PA610 40% glass fiber reinforced injection molding grade. Heat stabilized. Very high hydrolysis resistance. Black color. Suitable for parts requiring high stiffness, good mechanical resistance. Excellent retention of properties in contact with automotive cooling circuit liquids. This grade is partially renewable sourced (60% of base polymer by weight.)

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccDAM; ISO 1183
Water Absorption 1.9 %
@Thickness 2.00 mm,
Time 86400 sec
Immersion @ 23°C; ISO 62
Moisture Absorption 0.850 %
@Thickness 2.00 mm,
Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPa5mm / min. Conditioned; ISO 527-2/1A
 185 MPa5mm / min. DAM; ISO 527-2/1A
Elongation at Break 4.9 %5 mm / min. DAM; ISO 527-2/1A
 6.9 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 9800 MPa1mm / min. Conditioned; ISO 527-2/1A
 11500 MPa1mm / min. DAM; ISO 527-2/1A
Flexural Strength 280 MPa2mm / min. DAM; ISO 178
Flexural Modulus 10100 MPa2mm / min. DAM; ISO 178
Charpy Impact Unnotched 115 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 125 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 18.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 20.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohmDAM; 500V.; IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 217 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75/2Af
Flammability, UL94 HB
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 280 °CInjection Molding
Mold Temperature 80.0 - 90.0 °C
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6944 / 293449

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.