MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nevicolor NEVIMID 6 B E600 NC Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Polyamide 6, toughened

Information provided by Nevicolor

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm0.014 - 0.018 in/in115mm x 50mm x 3mm
Linear Mold Shrinkage, Transverse 0.014 - 0.108 cm/cm0.014 - 0.108 in/in115mm x 50mm x 3mm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ISO 868
Tensile Strength at Break 40.0 MPa5800 psiISO 527-1/2
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527-1/2
Elongation at Break >= 15 %>= 15 %ISO 527-1/2
Elongation at Yield 4.0 %4.0 %ISO 527-1/2
Modulus of Elasticity 2.20 GPa319 ksi1 mm/min; ISO 527-1/2
Flexural Strength 60.0 MPa8700 psi2 mm/min; ISO 178
Flexural Modulus 1.70 GPa247 ksiElastic; ISO 178
Izod Impact, Notched (ISO)  40.0 kJ/m²
@Temperature -20.0 °C
19.0 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) NBNBISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °F120°C/h; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °F120°C/h; ISO 75-1/-2
Vicat Softening Point  160 °C
@Load 5.10 kg
320 °F
@Load 11.2 lb
50°C/h; ISO 306/B
 210 °C
@Load 1.02 kg
410 °F
@Load 2.25 lb
50°C/h; ISO 306/A
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNEVI096 / 267440

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.