Description: The Chemlam® Silver series is the wear resistant line of Chemfab® industrial laminates. Chemlam® Silver composites feature uniform thickness, multi-layer cast PTFE films laminated to fiver glass reinforcements. Chemfab® laminates outperform traditional PTFE-coated products of similar weight and thickness. FEATURES: PTFE cast barrier film surface, crack and pinhole free: Outperforms simple PTFE-coated materials; long-lasting release properties make cleaning easier; low wicking of product into fabric extends useful life. Uniform film thickness over entire surface: Lamination eliminates the possibility of thin spots found in coated materials, which often lead to their premature failure. Bi-colored laminate: Attractive silver top surface is similar in appearance to PTFE cookware; natural (clear) rear surface can be used for inspection of belt condition and for backlighting through the belt. High temperature fabrics: Designed for thermal cycling and harsh chemical applications, including cooking and plastic processing. FDA Compliant: Suitable for use in direct food contact applications under the applicable requirements of 21CFR177.1550. All data based on a 0.0101 inch test sample. Information provided by Saint Gobain Performance Products. |