MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® 7109DL LLDPE Blown Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: This linear low density polyethylene is an ethylene-hexene copolymer tailored for blown film applications that require:
  • Good toughness properties
  • Good drawdown
  • Excellent processing characteristics
  • Use alone or in coextrusions; blends with other polyolefins
Typical blown film applications include:
  • Industrial films and bags
  • Thin gauge applications
  • General purpose packaging

Data provided by Chevron Phillips Chemical Company, LP.

Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Thickness 1.25 mil
Melt Flow 0.90 g/10 min190 °C/2.16 kg; ASTM D1238E
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 450 %ASTM D882
Film Elongation at Break, TD 650 %ASTM D882
Coefficient of Friction 0.50ASTM D1894
Elmendorf Tear Strength, MD 400 g/milASTM D1922
Elmendorf Tear Strength, TD 700 g/milASTM D1992
Dart Drop 275 g/milASTM D1709
Film Tensile Strength at Break, MD 8000 psiASTM D882
Film Tensile Strength at Break, TD 5000 psiASTM D882
1% Secant Modulus, MD 32000 psiASTM D882
1% Secant Modulus, TD 38000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 24 %ASTM D1003
Gloss 50 %60°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 204 °C
Die Opening 0.0762 cm
Extruder Size 6.35 cm
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade
LyondellBasell Petrothene® LP510300 High Density Polyethylene
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Data
Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin
Borealis Borstar® FB2230 LLDPE for Film

PCHEVF06 / 20267

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.