MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dynasol Solprene® 412 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Solprene 412 is a radial oil extended styrene butadiene block copolymer having 30% of styrene content, most of it forming a polystyrene block which gives the polymer a thermoplastic behavior. It is oil-extended with 6 phr of Paraffinic oil. It develops properties of vulcanized rubber yet not requiring vulcanization. It is protected with a non staining antioxidant system and is essentially gel free with a very clear color. Solprene 412 is used as elastomeric modifier for asphalt and in shoe sole compounding, injection molding and other thermoplastic crafts. It is available as free flowing pellets in standard paper bags, super-sacs and Gaylord boxes.

Information provided by Dynasol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccDIN 53479
Viscosity 25.38 cPToluene solution, 5.23%; NM 300-11
Brookfield Viscosity 18000 cP25%; ASTM D2994
Melt Index of Compound <= 0.50 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
Collected Volatile Condensable Material <= 1.0 %ASTM D1416
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79Shore A2; ASTM D2240
Tensile Strength at Break 14.4 MPaASTM D412
Elongation at Break 675 %ASTM D412
300% Modulus 0.00290 GPa
@Strain 300 %
ASTM D412
 
Descriptive Properties
Antioxidant Content1.1 %NM 300-52
Paraffinic Oil Content4-8 phrNM 300-54
PolystyreneMin 28 %NM 202-27

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Europrene® SOL TH 2314 Styrene - Ethylene / Butylene Block Copolymer
Dynasol Solprene® 4316 Thermoplastic Rubber (SBS)
Barlog Plastics KEBAFLEX S 45 A.01 TPE-S, Shore A45, translucent
Dynasol Solprene® 416 Thermoplastic Rubber SBS Dry
Kuraray SEPTON® S2004 Thermoplastic Rubber

PDYNA27 / 34775

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.