MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® MonoPlus SP 112 KR Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus SP 112 KR is a strongly acidic, premium grade, macroporous cation exchange resin with beads of uniform size (monodisperse) in highly regenerated form (min. 99% H) and purified (extremely low content of desorbable chloride ions) to meet nuclear industry specifications. Lewatit nuclear resins (Lewatit KR) are noted for their outstanding mechanical and chemical stability and their high osmotic stability. Because of their excellent hydrodynamic behavior, Lewatit KR resins allow particularly high flow rates. The extremely high monodispersity (uniformity coefficient: max 1.1) and very low fines content of max 0.1% (<0.315 mm) result in particularly low pressure losses compared with standard resins. Used in radioactive water circuits, they provide a number of special tasks and guarantee a water quality that fully complies with the requirements of the nuclear power industry. Lewatit MonoPlus SP 112 KR is particularly suitable for:
  • the removal of cations, including radioactive isotopes, from aqueous solutions (pH control through adsorption of excess 7-Li)
  • the decontamination of circuits in nuclear reactor plants
  • the removal of radioactive cations, highly selective for cesium 137
  • the treatment of primary coolant e.g. in pressure water reactors
  • purification of steam generator blow down irrespective of the conditioning with Levoxin (hydrazine), ethanolamine or morpholine
  • the removal of activated cleavage or corrosion products, including mechanical filtration of suspended impurities
  • the polishing in the primary and secondary sections as a mixed bed component with Lewatit MonoPlus M 800 KR or Lewatit MonoPlus MP 800 KR. Rinse carefully with demineralized water prior to service or mixing with Lewatit MonoPlus MP 800 KR or Lewatit MonoPlus M 800 KR.

    Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.740 g/cc
Density 1.18 g/cc
Bead Size 0.620 - 0.720 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceBeige-grey, opaque
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8803 / 209195

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.