MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Cerafelt Refractory Fiber Felt
Categories: Ceramic; Oxide

Material Notes: Cerafelt™ is an insulating refractory felt, obtained by hot pressing. It is made from Cerachem fibers, bonded with an organic binder which begins to burn out at 180°C. This special binder makes Cerafelt particularly suitable for die-cutting operations. Semi rigid, it is neither brittle nor dusty. Cerafelt optimizes the manufacture of complex, die-cut shapes to close tolerances. With a choice from eight densities and seven thicknesses, Cerafelt offers a grade to suit most requirements. Made from chemically stables fibers, lightweight and very insulating, Cerafelt is a multi-purpose product.

Applications:

  • High temperature gaskets
  • Expansion joints for furnace, kiln and boiler linings
  • Die cut shapes for domestic appliances
  • Thermal barrier media
  • Insulating thermal break

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0480 - 0.384 g/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0600 W/m-K
@Temperature 300 °C
at 384kg/m3; NFS-40-456
 0.0700 W/m-K
@Temperature 300 °C
at 160 kg/m3; NFS-40-456
 0.0700 W/m-K
@Temperature 300 °C
at 192 kg/m3; NFS-40-456
 0.0700 W/m-K
@Temperature 300 °C
at 288 kg/m3; NFS-40-456
 0.0800 W/m-K
@Temperature 300 °C
at 128 kg/m3; NFS-40-456
 0.100 W/m-K
@Temperature 300 °C
at 64kg/m3; NFS-40-456
 0.110 W/m-K
@Temperature 300 °C
at 48kg/m3; NFS-40-456
 0.130 W/m-K
@Temperature 700 °C
at 384kg/m3; NFS-40-456
 0.130 W/m-K
@Temperature 700 °C
at 288 kg/m3; NFS-40-456
 0.150 W/m-K
@Temperature 700 °C
at 192 kg/m3; NFS-40-456
 0.160 W/m-K
@Temperature 700 °C
at 160 kg/m3; NFS-40-456
 0.180 W/m-K
@Temperature 1000 °C
at 384kg/m3; NFS-40-456
 0.210 W/m-K
@Temperature 1000 °C
at 288 kg/m3; NFS-40-456
 0.210 W/m-K
@Temperature 700 °C
at 128 kg/m3; NFS-40-456
 0.250 W/m-K
@Temperature 1000 °C
at 192 kg/m3; NFS-40-456
 0.270 W/m-K
@Temperature 700 °C
at 64kg/m3; NFS-40-456
 0.290 W/m-K
@Temperature 1000 °C
at 160 kg/m3; NFS-40-456
 0.330 W/m-K
@Temperature 700 °C
at 48kg/m3; NFS-40-456
 0.420 W/m-K
@Temperature 1000 °C
at 128 kg/m3; NFS-40-456
 0.590 W/m-K
@Temperature 1000 °C
at 64kg/m3; NFS-40-456
 0.750 W/m-K
@Temperature 1000 °C
at 48kg/m3; NFS-40-456
Shrinkage 2.5 %
@Temperature 1260 °C,
Time 86400 sec
permanent, at isothermal; NFB-40-456
 3.0 %
@Temperature 1320 °C,
Time 86400 sec
permanent, at isothermal; NFB-40-456
 
Component Elements PropertiesOriginal ValueComments
Al2O3 35.1 %
CaO+MgO 0.050 %
Fe2O3 0.10 %
K2O+Na2O 0.20 %
Loss on Ignition(%) 4.0 - 12 %
SiO2 49.7 %
ZrO2 14.7 %
 
Descriptive Properties
Classification Temperature (°C)1320
Coloryellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool A Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 80 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 3000 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic

CMORF7064 / 203363

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.