MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lanxess LEWATIT® MonoPlus TP 214 Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus TP 214 is monospherical, macroporous, chelating resin with thiourea groups having a high affinity for mercury. Next to this special mercury selectivity. Lewatit MonoPlus TP 214 has a high selectivity for PGM metals such as platinum, gold and silver. For these reasons, it is specially used for
  • the removal of mercury in flue gas scrubbing processes
  • the removal of mercury from brines in front of chloralkali membrane processes and effluents from chloralkali electrolysis plants using mercury process
  • the removal of mercury from ground water
  • metal separation and recovery in hydrometallurgy
  • the recovery of PFM-metals from rinse water and exhausted process solutions
  • recovery of palladium catalysis from organic process streams
Cations are removed from solutions in the following order: Hg2>Ag>Au1/3>Pt2/4> Cu2>Pb2/4>Bi2>Sn2>Zn2>Cd2>Ni2 Based on more than 25 years of experience with the old replaced heterodispersed Lewatit TP 214, this new resin, produced by a new patented process, offers clear advantages:
  • a higher mechanical and osmotic stability
  • better kinetics
  • a 10-20% higher capacity, depending on process conditions
  • a remarkable low leakage according to the process conditions
The regeneration of Lewatit MonoPlus TP 214 exhausted with mercury is not possible with usually applied regenerant solutions. Therefore, exhausted resins can only be disposed in accordance with the local regulations governing their disposal. The regeneration of Lewatit Monoplus TP 214 exhausted with precious metal sin general is not possible. The recovery of these metals is usually practiced by incineration in special designed furnaces. The regeneration of Lewatit MonoPlus TP 214 loaded with Zn2, Cd2, Ni2, Pb2, Cu2, is partially possible but connected with intellectual properties of third parties.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.680 g/cc0.0246 lb/in³
Density 1.10 g/cc0.0397 lb/in³
Bead Size 0.500 - 0.600 mm0.0197 - 0.0236 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceBeige, opaque
pH Operating Range4 - 10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium (IV) Oxide, TiO2
Titanium Dioxide, Brookite
Momentive Performance Materials HPC Boron Nitride (BN)/TiO2 Water Based Coating
Hafnium Oxide, HfO2
Hafnium (II) Oxide, HfO2 (Hafnia)

PLANY8808 / 209200

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.