MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Guang Dong Glass Fiber Reinforced PA
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Application Field: Suitable for machinery spare parts, auto parts, electronics & electrical industry, railway, communication and sports products industry, gears, axle sleeve

Feature: Good comprehensive performance, high strength, high rigidity and hardness, creep resistance, heat aging resistance, excellent processing performance

Information provided by GuangDong LuHua New Material Technology Holding Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 101101ASTM D785
Tensile Strength 195 MPa28300 psiASTM D638
Elongation at Break 3.0 - 3.5 %3.0 - 3.5 %ASTM D638
Flexural Strength 240 - 262 MPa34800 - 38000 psiASTM D790
Flexural Modulus 8.963 GPa1300 ksiASTM D790
Izod Impact, Notched (ISO) 0.100 - 0.150 kJ/m²0.0476 - 0.0714 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 248 - 253 °C478 - 487 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGDON023 / 283971

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.