MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ConocoPhillips Hydroclear® 68 Multi-Way Machine Lubricant
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Multi-Way Machine Lubricant is a high-quality, heavy-duty circulating machine tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Multi-Way Machine Lubricant is specially formulated with proprietary additive chemistry containing oiliness and tackiness agents and is recommended for use on the plain bearing slideways of lathes, shapers, grinders, milling machines and other machine tools. Hydroclear Multi-Way Machine Lubricant also can be used effectively on the slideways of saws and carriages found in lumber mills. Hydroclear Multi-Way Machine Lubricant has exceptional stick/slip properties to prevent problems during slow-speed operations. Hydroclear Multi-Way Machine Lubricant provides exceptional control of lubricant runoff, excellent adhesion to horizontal and vertical way surfaces, good rust and corrosion protection and wear protection. Hydroclear Multi-Way Machine Lubricant is available in ISO viscosity grades 68 and 220. Hydroclear Multi-Way Machine Lubricant has been tested and formally approved by Cincinnati Milacron in accordance with its Lubricant Specifications.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.36 lb/gal
Viscosity Measurement 110Viscosity Index
Saybolt Viscosity at 100°F 365 SUS
Saybolt Viscosity at 210°F 58 SUS
Kinematic Viscosity at 40°C (104°F) 70 cSt
Kinematic Viscosity at 100°C (212°F) 9.5 cSt
ASTM Color 1.0
 
Thermal PropertiesOriginal ValueComments
Pour Point 5.00 °F
Flash Point 450 °F
 
Descriptive Properties
Stick/Slip Ratio0.6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON107 / 75144

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.