MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

TOSAF Compounds Tosaf UV 5925 PE PE, Masterbatch
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: UV absorber masterbatch, to be used in LDPE, LLDPE, HDPE, PP and EMA films and packaging. UV absorber masterbatch to be used in films protects the final products against decomposition due to light exposure and Food packaging produced using this MB inhibit UVA radiation from penetrating through to the content of the package.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additives Category: Masterbatch – UV Protector/Light Stabilizer – UV Absorber

Carrier Resin: Polyethylene or ethylene-olefin copolymer (PE)

Recommended for Use In: Polyethylene or ethylene-olefin copolymer (PE); Polypropylene or propylene-olefin copolymer (PP)

Form: Pellets/Granules

State at Room Temperature: Solid

Information provided by TOSAF Compounds Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.450 - 0.610 g/cc0.0163 - 0.0220 lb/in³
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Descriptive Properties
Additive Concentration0.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTOSAF1517 / 312210

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.