System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Petropol Thanelene® A3 80A HL PRTA010 TP307 MSP TPU
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Product Description: Hardness 80 shore A, Free from plasticizers, Thermoplastic Polyurethane
Resin ID (ISO 1043): TPU
Additive: Plasticized
Processing: Injection Molding, Extrusion
Color: Black
Information provided by Petropol
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.20
g/cc
DIN 53479
Mechanical Properties
Original Value
Comments
Hardness, Shore A
80
DIN 53505
Tensile Strength, Ultimate
>=
30.0
MPa
DIN 53504
Tensile Stress
1.30
MPa
@Strain 10 %
DIN 53504
3.30
MPa
@Strain 50 %
DIN 53504
4.10
MPa
@Strain 100 %
DIN 53504
7.60
MPa
@Strain 300 %
DIN 53504
Elongation at Break
>= 700 %
DIN 53504
Resilience
44
[%], Impact Resilience; ISO 4662
Tear Strength
56.0
kN/m
Propagation; ISO 34-1
Abrasion
<= 35
[mm3]; ISO 4649/A
Compression Set
22 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
39 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
Processing Properties
Original Value
Comments
Mold Temperature
180
-
200
°C
Drying Temperature
80.0
°C
Dry Time
3.00
-
4.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PPETROPOL402 / 313310
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.