MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos K44-11-128 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. This material combines excellent processability and environmental stress crack resistance (ESCR) with well-balanced end use properties. This resin meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Outstanding physical performance and low color
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.947 g/ccASTM D4883
High Load Melt Index 12 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ASTM D2240
Tensile Strength, Yield 23.8 MPa2 in/min (50 mm/min); ASTM D638
Elongation at Break 850 %2 in/min (50 mm/min); ASTM D638
Flexural Modulus 0.579 GPaASTM D747
 0.841 GPa
@Strain 2 %
Secant-Method 1; ASTM D790
Izod Impact, Notched 4.70 J/cmPartial break; ASTM D256
Tensile Impact Strength 710 kJ/m²ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °CASTM D648
Vicat Softening Point 129 °CASTM D1525
Brittleness Temperature <= -75.0 °CASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
processBlow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Paxon™ BA50-100 Blow Molding Resin
LyondellBasell Alathon® M5370 High Density Polyethylene
Ineos G60-25-144 HDPE
Ineos G36-24-150 HDPE
Ineos K50-10-136 HDPE

PSOLJI / 68188

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.