Physical Properties | Metric | English | Comments |
---|
Density | 0.219 - 0.409 g/cc | 0.00793 - 0.0148 lb/in³ |
Water Absorption | <= 4.4 % | <= 4.4 % |
Absorption Coefficient | 0.15 @Thickness 6.00 mm | 0.15 @Thickness 0.236 in |
| 0.40 @Thickness 10.0 mm | 0.40 @Thickness 0.394 in |
| 0.60 @Thickness 15.0 mm | 0.60 @Thickness 0.591 in |
| 0.70 @Thickness 25.0 mm | 0.70 @Thickness 0.984 in |
| 0.010 @Thickness 6.00 mm, Frequency 125 Hz | 0.010 @Thickness 0.236 in, Frequency 125 Hz |
| 0.010 @Thickness 10.0 mm, Frequency 125 Hz | 0.010 @Thickness 0.394 in, Frequency 125 Hz |
| 0.030 @Thickness 6.00 mm, Frequency 250 Hz | 0.030 @Thickness 0.236 in, Frequency 250 Hz |
| 0.030 @Thickness 15.0 mm, Frequency 125 Hz | 0.030 @Thickness 0.591 in, Frequency 125 Hz |
| 0.040 @Thickness 10.0 mm, Frequency 250 Hz | 0.040 @Thickness 0.394 in, Frequency 250 Hz |
| 0.070 @Thickness 6.00 mm, Frequency 500 Hz | 0.070 @Thickness 0.236 in, Frequency 500 Hz |
| 0.090 @Thickness 25.0 mm, Frequency 125 Hz | 0.090 @Thickness 0.984 in, Frequency 125 Hz |
| 0.11 @Thickness 15.0 mm, Frequency 250 Hz | 0.11 @Thickness 0.591 in, Frequency 250 Hz |
| 0.15 @Thickness 10.0 mm, Frequency 500 Hz | 0.15 @Thickness 0.394 in, Frequency 500 Hz |
| 0.18 @Thickness 6.00 mm, Frequency 1000 Hz | 0.18 @Thickness 0.236 in, Frequency 1000 Hz |
| 0.28 @Thickness 25.0 mm, Frequency 250 Hz | 0.28 @Thickness 0.984 in, Frequency 250 Hz |
| 0.38 @Thickness 15.0 mm, Frequency 500 Hz | 0.38 @Thickness 0.591 in, Frequency 500 Hz |
| 0.39 @Thickness 6.00 mm, Frequency 2000 Hz | 0.39 @Thickness 0.236 in, Frequency 2000 Hz |
| 0.46 @Thickness 10.0 mm, Frequency 1000 Hz | 0.46 @Thickness 0.394 in, Frequency 1000 Hz |
| 0.74 @Thickness 6.00 mm, Frequency 4000 Hz | 0.74 @Thickness 0.236 in, Frequency 4000 Hz |
| 0.77 @Thickness 25.0 mm, Frequency 500 Hz | 0.77 @Thickness 0.984 in, Frequency 500 Hz |
| 0.80 @Thickness 15.0 mm, Frequency 1000 Hz | 0.80 @Thickness 0.591 in, Frequency 1000 Hz |
| 0.87 @Thickness 10.0 mm, Frequency 2000 Hz | 0.87 @Thickness 0.394 in, Frequency 2000 Hz |
| 0.89 @Thickness 15.0 mm, Frequency 4000 Hz | 0.89 @Thickness 0.591 in, Frequency 4000 Hz |
| 0.90 @Thickness 25.0 mm, Frequency 4000 Hz | 0.90 @Thickness 0.984 in, Frequency 4000 Hz |
| 0.94 @Thickness 25.0 mm, Frequency 2000 Hz | 0.94 @Thickness 0.984 in, Frequency 2000 Hz |
| 0.94 @Thickness 10.0 mm, Frequency 4000 Hz | 0.94 @Thickness 0.394 in, Frequency 4000 Hz |
| 1.03 @Thickness 15.0 mm, Frequency 2000 Hz | 1.03 @Thickness 0.591 in, Frequency 2000 Hz |
| 1.03 @Thickness 25.0 mm, Frequency 1000 Hz | 1.03 @Thickness 0.984 in, Frequency 1000 Hz |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength | 0.0703 - 0.190 MPa | 10.2 - 27.6 psi |
Elongation at Break | 50 - 90 % | 50 - 90 % |
Tear Strength | 0.400 - 1.40 kN/m | 2.28 - 7.99 pli |
|
Thermal Properties | Metric | English | Comments |
---|
Thermal Conductivity | <= 0.0620 W/m-K @Temperature 0.000 °C | <= 0.430 BTU-in/hr-ft²-°F @Temperature 32.0 °F |
Maximum Service Temperature, Air | 85.0 °C | 185 °F |
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F |
|
Processing Properties | Metric | English | Comments |
---|
Shelf Life | 36.0 Month | 36.0 Month |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.