MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Corbion Purac Blend A High Heat Homopolymer PLA
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Data is for samples produced from Puralact L and D lactide monomers; Purac also produces high stereo optical purity lactide monomers. PLA is 100% biobased and is both recyclable and compostable. PLA can be used in a broad range of applications from molded plastic parts to textiles, foams, and films.

Information provide by Corbion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45.0 MPa
Elongation at Break 5.0 %
Tensile Modulus 3.00 GPa
Charpy Impact, Notched 0.500 J/cm²
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °CHDT B flatwise
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 220 °Cpre-drying required
Mold Temperature 80.0 - 100 °C
 
Descriptive Properties
ClarityNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corbion Purac Blend C High Heat, Impact Modified Homopolymer PLA
Corbion Purac Blend B High Heat, High Modulus Homopolymer PLA
NatureWorks® Ingeo™ 3801X Injection Grade PLA
NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer

PPURAC90 / 133272

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.