MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Seals Eastern 7336 Highly Saturated Nitrile Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: HNBR for Oil & Gas service

Information provided by Seals Eastern, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D297, 15
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 77ASTM D2240, Type A
 80AVG; ASTM D2240, Type A
 82
@Treatment Temp. 100 °C,
Time 252000 sec
After Dry Heat Aging; ASTM D865
 82
@Treatment Temp. 100 °C,
Time 605000 sec
After Dry Heat Aging; ASTM D865
 84
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
After Dry Heat Aging; ASTM D865
 84
@Treatment Temp. 100 °C,
Time 3.60e+6 sec
After Dry Heat Aging; ASTM D865
Tensile Strength at Break >= 3565 psiASTM D412 Method A
 3645 psiAVG; ASTM D412 Method A
 3135 psi
@Treatment Temp. 100 °C,
Time 605000 sec
After Dry Heat Aging; ASTM D865
 3149 psi
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
After Dry Heat Aging; ASTM D865
 3175 psi
@Treatment Temp. 100 °C,
Time 252000 sec
After Dry Heat Aging; ASTM D865
 3273 psi
@Treatment Temp. 100 °C,
Time 3.60e+6 sec
After Dry Heat Aging; ASTM D865
Tensile Stress at Strain 285 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 370 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 380 psi
@Strain 50 %
Average; ASTM D412 Method A
 >= 715 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 735 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 290 %ASTM D412 Method A
 295 %AVG; ASTM D412 Method A
 185 %
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
After Dry Heat Aging; ASTM D865
 195.6 %
@Treatment Temp. 100 °C,
Time 3.60e+6 sec
After Dry Heat Aging; ASTM D865
 204 %
@Treatment Temp. 100 °C,
Time 605000 sec
After Dry Heat Aging; ASTM D865
 206 %
@Treatment Temp. 100 °C,
Time 252000 sec
After Dry Heat Aging; ASTM D865
Modulus of Elasticity 2.00 ksiASTM D412 Method A
Poissons Ratio 0.49Calculated
Shear Modulus 0.670 ksiASTM D412 Method A
Secant Modulus 1.90 ksiASTM D412 Method A
Tear Strength Test 570(psi); ASTM D624, Die B
Compression Set 33 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395, Test B
 37.5 %
@Temperature 100 °C,
Time 252000 sec
ASTM D395, Test B
 54 %
@Temperature 100 °C,
Time 1.21e+6 sec
ASTM D395, Test B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °FASTM D1329
Glass Transition Temp, Tg -1.00 °FASTM D1329
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QM 258 60 Shore A, Addition Cure Moldmaking Material
Seals Eastern 7202 Nitrile Rubber
Garlock 502 Silicone Sheet Rubber
KKPC KOSYN KNB 25LM Acrylonitrile Butadiene Rubber (NBR)
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III

PSEAL16 / 80163

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.