MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Parker Chomerics SOFT-SHIELD® 3500 Plated-Fabric Wrapped Foam Economical EMI Shielding Gasket for Electronics
Categories: Polymer

Material Notes: Description: The SOFT-SHIELD® 3500 fabric cover foam [FOF] product family is a group of low-closure force EMI/EMC gaskets. SS3500 offers a low cost/ low closure force competitive solution for EMI shielding and electrical grounding in shear and compression. The SS3500 product family is comprised of conductive fabric wrapped around open cell foam. This wrap around technology grounds the gasket from point to point, ultimately eliminating an EMI/EMC gap.

Typical Applications: Server Faceplates and blade cards; Electronic enclosures; Consumer electronics; Door seals; EMI Window/vent seals and Grounding Applications.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Deformation 35 %35 %<1 ppi, .105" x .5" gasket; ASTM C165
 30 - 60 %30 - 60 %Recommended
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.700 kN/m3.99 pli90° Acrylic Adhesive; ASTM D1000
Compression Set <= 15 %<= 15 %ASTM D3574
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness >= 100 dB
@Frequency 5.00e+7 - 1.00e+10 Hz
>= 100 dB
@Frequency 5.00e+7 - 1.00e+10 Hz
CHO-TM-TP08
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schmolz + Bickenbach UGICHROM 4021 Martensitic Chrome Plated Bar
Schmolz + Bickenbach UGICHROM 4305 Austenitic Chrome Plated Bar
Schmolz + Bickenbach UGICHROM 4057 Martensitic Chrome Plated Bar
Schmolz + Bickenbach UGICHROM 4028 Martensitic Chrome Plated Bar
Schmolz + Bickenbach UGICHROM 244 Chrome Plated Bar

PCHOME264 / 130974

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.