System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Encom Polymers EnLast 75A TPV
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Thermoplastic Vulcanizate Elastomer (TPV)
Material Notes:
Appearance: Black
Processing Methods: Injection Molding
Applications: Automotive, Appliance, General Industrial
Information provided by EnCom Polymers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.02
g/cc
Method A; ISO 1183
Mechanical Properties
Original Value
Comments
Hardness, Shore A
75
15 sec delay; ISO 868
81.75
1008 Hours at 100°C in an air circulating oven followed by indicated property testing at 23°C; ISO 188
Tensile Strength, Yield
5.00
MPa
Type 1, 50mm/min; ISO 37
5.05
MPa
1008 Hours at 100°C in an air circulating oven followed by indicated property testing at 23°C; ISO 188
Elongation at Break
356 %
1008 Hours at 100°C in an air circulating oven followed by indicated property testing at 23°C; ISO 188
400 %
Type 1, 50mm/min; ISO 37
Tear Strength
26.0
kN/m
Method B, Procedure b, 50mm/min; ISO 34-1
Processing Properties
Original Value
Comments
Rear Barrel Temperature
320
-
360
°F
Middle Barrel Temperature
340
-
380
°F
Front Barrel Temperature
360
-
400
°F
Nozzle Temperature
360
-
400
°F
Melt Temperature
380
-
400
°F
Mold Temperature
90.0
-
160
°F
Back Pressure
25.0
-
100
psi
Vent Depth
0.000500
-
0.00150
in
Screw Speed
25
-
75
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PENCOM216 / 266230
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.