Aqueous dispersion, 175 ml
Concentration: 500 mg/L
Composition: Carbon (79%), Oxygen (20%)
Flake size: 0.3-0.7 microns
Thickness: 1 atomic layer - at least 80%.
Color:BrownApplication: Graphene-polymer composite materials
Ultrastrong graphene oxide paper
Transparent conductive coatings
Solar cells
Supercapacitors
Support for metaliic catalysts
Low permeability materials
Electro-static Dissipation (ESD) films
Chemical and bio sensors
Multifunctional Materials Based on Graphene
Graphene Research |