Hostacom 0207 8049 (U024) is an unfilled polypropylene copolymer, with very high melt flow rate offering a good impact/stiffness balance. Product is available as a customized color matched, pellet form. This grade is delivered in 8049 color version. Applications: Interior Automotive Applications.Information provided by LyondellBasell. |