MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Neoprene WRT-M1 Polychloroprene Rubber  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Neoprene Type WRT-M1 is a polychloroprene/2,3 dichloro 1,3-butadiene copolymer, has excellent polymer stability, and a very slow crystallization rate. Physical form: Chips. Color: White to Silver Gray. Distinguishing Features: Low-viscosity WRT.

Neoprene W-type Characteristics: Raw polymers: Excellent storage stability; non-peptizable; accelerator required/cure flexibility. Vulcanizates: Best compression set resistance, best heat-aging.

General Neoprene Information: The basic chemical structure of DuPont Dow Elastomers Neoprene is polychloroprene. The polymer structure can be modified by copolymerization with sulfur or 2,3 dichloro 1,3-butadiene to yield a broad range of chemical and physical properties. All types of Neoprene resist degradation from sun, ozone, and weather; perform well in contact with oils and many chemicals; remain useful over a wide temperature range; display outstanding physical toughness, and resist burning inherently better than exclusively hydrocarbon rubbers.

Information provided by DuPont Dow Elastomers.

Denka Performance Elastomer LLC has acquired the Neoprene product line from DuPont Performance Polymers. This specific product had already been discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³
Mooney Viscosity 34 - 42
@Temperature 100 °C
34 - 42
@Temperature 212 °F
ML 1+4; ASTM D1646-81

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polychloroprene Rubber (CR)
Armacell Monarch® F-02001 Neoprene Based Rubber Foam
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
DuPont Mobility and Materials Neoprene FB Polychloroprene Rubber
Eurofoam Porocell POR 303/B CR-Neoprene/NBR Foam

PDVE09 / 34051

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.