MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Qualchem Danamid FGF-20 Polyamide 6, 20% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Reinforced with glass fiber.

Information provided by Qualchem Zrt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccDIN 53479
Filler Content 18 - 22 %
Moisture Absorption at Equilibrium 2.0 - 2.2 %DIN 53714
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 110 MPa50 mm/min; ISO 527-1,2
Elongation at Break 4.0 %ISO 527-1,2
Tensile Modulus 5.70 GPaISO 527-1,2
Flexural Strength 200 MPa10mm/min; DIN 53452
Charpy Impact Unnotched >= 2.00 J/cm²
@Temperature 23.0 °C
DIN 53453
Charpy Impact, Notched >= 0.500 J/cm²
@Temperature 23.0 °C
DIN 53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDIN 53482
Comparative Tracking Index 550 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 190 °CDIN 53461
Flammability, UL94 HB
@Thickness 4.00 mm
MSZ 10383

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PQUALC33 / 58445

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.