MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotch® 393 General Purpose Cloth Tape
Categories: Polymer; Adhesive

Material Notes: Scotch® General Purpose Cloth Tape 393 is a polyethylene coated cloth backing coated with a rubber adhesive for moisture-proofing, duct sealing and general purpose applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 305 microns12.0 milASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 21.1 MPa3050 psiASTM D3756
Elongation at Break 8.0 %8.0 %ASTM D3756
Peel Strength 1.0408 kN/m5.9375 plito Steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Adhesive TypeRubber
AppearanceSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch® 231A Performance Masking Tape
3M Scotch® 231 Performance Masking Tape
3M Scotch® 226 Solvent Resistant Masking Tape
3M Scotch® 222 High-temperature Fine Line Masking Tape
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape

PMM33974 / 168721

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.