MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wacker Silres® BS 3003 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: SILRES® BS 3003 is a water-thinnable, solventless emulsion, based on a mixture of silane and siloxane. Dilute solutions of SILRES® BS 3003 serve as high quality, general-purpose water repellents for impregnating and priming mineral surfaces. Moreover SILRES® BS 3003 can be used for the mass treatment of non-load bearing concrete products.

Properties: SILRES® BS 3003 emulsion contains a stabilized mixture of silanes and siloxanes that are susceptible to hydrolysis. Hydrolysis occurs only after application to the substrate, which breaks the emulsion. Alcohol is released and the emulsion is converted into a silicone resin water repellent. SILRES® BS 3003 reduces the capillary absorption of the building which it has penetrated, but does not clog pores or capillaries. There is therefore little or no impairment of the building material´s ability to "breathe".

Special features: SILRES® BS 3003 shows the following special features:

  • good depth of penetration
  • resistance to alkalis
  • rapid development of water repellency
  • provides good adhesion for paints
  • water based and environmentally friendly
  • stable in storage, even when diluted

    Application: Dilute SILRES® BS 3003 is an excellent water repellent for many absorbent mineral substrates, such as bricks, sand-lime brick, natural sandstone and mineral plasters. It is not so suitable for less absorbent, dense natural stone, especially limestone, marble and reinforced concrete for bridges and roads. Owing to its aqueous consistency and storage stability when diluted, SILRES® BS 3003 is ideal for inplant impregnation of building materials made of clay, aerated concrete, sand-lime brick, fibrous cement, mineral fibers and lightweight aggregate. SILRES® BS 3003 may also serve as a water-repellent primer for emulsion paints and plasters, silicone resin emulsion paints and silicone resin plasters. Moreover SILRES® BS 3003 can be used for the mass treatment of non-load bearing concrete products.

    Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³
pH 8.08.0
Viscosity 12 cP12 cPdynamic
 
Descriptive Properties
Active ingredients (%)60
Appearancemilky, white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9556 / 205085

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.