MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 2330 Steel (UNS G23300)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Key Words: UNS G23300
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 248
Tensile Strength, Ultimate 841 MPa
Tensile Strength, Yield 689 MPa
@Strain 0.2 %
Elongation at Break 19 %
Modulus of Elasticity 201 - 209 GPa
Bulk Modulus 160 - 170 GPa
Poissons Ratio 0.27 - 0.30
Shear Modulus 81.0 - 82.0 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.9 µm/m-°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 2515 Steel (UNS G25150)
AISI 1335 Steel
AISI 3120 Steel (UNS G31200)
AISI 3150 Steel (UNS G31500)
Overview of materials for AISI 4000 Series Steel

M2330 / 100228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.