MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nanocyl PLASTICYL™ PA1503 Polyamide 6 with 1 wt% of Multi-Wall Carbon Nanotubes
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PA1503 is a conductive masterbatch based on polyamide 6. Because of its high flow formulation, PLASTICYL™ PA1503 is ideal for standard injection molding and extrusion processes.

Applications:

  • ESD (Electrostatic Discharge) and electrically conductive parts
  • E&E, automotive, industrial
  • Injection molding, extrusion

Benefits:

  • Electrical conductivity at low loading
  • Retention of key mechanical properties
  • Easier processing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 1 %Carbon Nanotube Loading
Melt Flow 42.48 g/10 min
@Load 1.20 kg,
Temperature 280 °C
ISO 1133:1997
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+8 ohm-cmApproximate value obtained from graph; CTM E043
Surface Resistivity per Square 6.00e+12 ohmApproximate value obtained from graph; CTM E042
 
Thermal PropertiesOriginal ValueComments
Melting Point 221 °CMasterbatch; ISO 11357-1,-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced
Hexcel® HexForce™ SGP203-CS Carbon Fabric
Hexcel® HexForce™ 284 Carbon Fabric

PNANOCY983 / 108938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.