Heat stabilizer for rigid and flexible formulation.Excellent clarity,lubricity,and weathering stability.synergistic heat stabilizer and lubricant used in combination with organotin maleate or mercaptides in rigid PVC. Information provided by Pau Tai Industrial Corp. |
Dibutyl Tin Dilaurate organic complex |