MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Global PP-1102-K Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description-transparency, high stiffness, high heat resistant
Applications-textile applications, bags, tape, sheet

Information provided by Global Polymers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 88.0 MPaDIN 53456
Tensile Strength, Yield 5080 psiASTM D638
Shear Modulus 0.700 GPaDIN 53457
Charpy Impact, Notched 0.370 J/cm²
@Temperature -23.0 °C
DIN 53453
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 230 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene Copolymer
Phillips 66 COPYLENE® CR020CL Polypropylene Impact Copolymer
Phillips 66 COPYLENE® CM090L Polypropylene, High Impact Copolymer
Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming
Phillips 66 COPYLENE® CM020N Polypropylene Impact Copolymer

PGLOBP09 / 42110

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.