Vydyne 909 is an halogenated, 25% glass filled, flame retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4mm (0.016") thick.Information provided by Ascend Performance Materials. |