MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type S24100 Stainless Steel 25 mm mill-annealed bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Low nickel, austenitic with comparable corrosion resistance, high work hardenability permits cold drawing to high-strength levels while maintaining good ductility, excellent wear- and galling-resistance, resists staining and rusting in 5% sodium chloride fog and high-humidity atmospheres, readily welded. Applications include high-strength shafting and bolting, clamps for pole line hardware, concrete reinforcing accessories, abrasion and corrosion resistant screens, high-strength nonmagnetic springs, wire forms, racks and cages.

Key Words: UNS S24100, ASTM A276 (XM-28), ASTM A313 (XM-28), ASTM A580 (XM-28)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.78 g/cc0.281 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 814 MPa118000 psi
 345 MPa
@Temperature 760 °C
50000 psi
@Temperature 1400 °F
 455 MPa
@Temperature 650 °C
66000 psi
@Temperature 1200 °F
 525 MPa
@Temperature 540 °C
76100 psi
@Temperature 1000 °F
 570 MPa
@Temperature 425 °C
82700 psi
@Temperature 797 °F
 615 MPa
@Temperature 315 °C
89200 psi
@Temperature 599 °F
 650 MPa
@Temperature 205 °C
94300 psi
@Temperature 401 °F
 717 MPa
@Temperature 95.0 °C
104000 psi
@Temperature 203 °F
Tensile Strength, Yield 485 MPa
@Strain 0.2 %
70300 psi
@Strain 0.2 %
 200 MPa
@Strain 0.2 %,
Temperature 760 °C
29000 psi
@Strain 0.2 %,
Temperature 1400 °F
 215 MPa
@Strain 0.2 %,
Temperature 650 °C
31200 psi
@Strain 0.2 %,
Temperature 1200 °F
 235 MPa
@Strain 0.2 %,
Temperature 540 °C
34100 psi
@Strain 0.2 %,
Temperature 1000 °F
 250 MPa
@Strain 0.2 %,
Temperature 425 °C
36300 psi
@Strain 0.2 %,
Temperature 797 °F
 270 MPa
@Strain 0.2 %,
Temperature 315 °C
39200 psi
@Strain 0.2 %,
Temperature 599 °F
 305 MPa
@Strain 0.2 %,
Temperature 205 °C
44200 psi
@Strain 0.2 %,
Temperature 401 °F
 395 MPa
@Strain 0.2 %,
Temperature 95.0 °C
57300 psi
@Strain 0.2 %,
Temperature 203 °F
Elongation at Break 53 %53 %Gage length is 4 times specimen diameter.
 31 %
@Temperature 760 °C
31 %
@Temperature 1400 °F
Gage length is 4 times specimen diameter.
 39 %
@Temperature 650 °C
39 %
@Temperature 1200 °F
Gage length is 4 times specimen diameter.
 47 %
@Temperature 540 °C
47 %
@Temperature 1000 °F
Gage length is 4 times specimen diameter.
 50 %
@Temperature 205 °C
50 %
@Temperature 401 °F
Gage length is 4 times specimen diameter.
 50 %
@Temperature 315 °C
50 %
@Temperature 599 °F
Gage length is 4 times specimen diameter.
 50 %
@Temperature 425 °C
50 %
@Temperature 797 °F
Gage length is 4 times specimen diameter.
 52 %
@Temperature 95.0 °C
52 %
@Temperature 203 °F
Gage length is 4 times specimen diameter.
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
Machinability 30 %30 %Based on 100% machinability for AISI 1212 steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000660 ohm-cm0.0000660 ohm-cmTypical value for stainless steel.
Magnetic Permeability 1.0081.008H = 200 Oe, annealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.2 µm/m-°C
@Temperature 24.0 - 95.0 °C
9.00 µin/in-°F
@Temperature 75.2 - 203 °F
 16.9 µm/m-°C
@Temperature 24.0 - 205 °C
9.39 µin/in-°F
@Temperature 75.2 - 401 °F
 17.6 µm/m-°C
@Temperature 24.0 - 315 °C
9.78 µin/in-°F
@Temperature 75.2 - 599 °F
 18.0 µm/m-°C
@Temperature 24.0 - 425 °C
10.0 µin/in-°F
@Temperature 75.2 - 797 °F
 18.5 µm/m-°C
@Temperature 24.0 - 540 °C
10.3 µin/in-°F
@Temperature 75.2 - 1000 °F
 19.3 µm/m-°C
@Temperature 24.0 - 650 °C
10.7 µin/in-°F
@Temperature 75.2 - 1200 °F
 19.8 µm/m-°C
@Temperature 24.0 - 760 °C
11.0 µin/in-°F
@Temperature 75.2 - 1400 °F
 20.2 µm/m-°C
@Temperature 24.0 - 870 °C
11.2 µin/in-°F
@Temperature 75.2 - 1600 °F
 20.9 µm/m-°C
@Temperature 24.0 - 980 °C
11.6 µin/in-°F
@Temperature 75.2 - 1800 °F
Specific Heat Capacity 0.480 J/g-°C0.115 BTU/lb-°FTypical value for stainless steel.
Thermal Conductivity 20.7 W/m-K144 BTU-in/hr-ft²-°FTypical value for stainless steel.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 18 %18 %
Iron, Fe 66 %66 %
Manganese, Mn 13 %13 %
Nickel, Ni 1.5 %1.5 %
Nitrogen, N 0.33 %0.33 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S24100 Stainless Steel 25 mm annealed bar at RT
302 Stainless Steel, 60% cold reduction
AISI Type S24100 Stainless Steel 6.4 mm diameter annealed rod, 60% cold reduction
ATI Allvac® REX 734™ UNS S31675 Specialty Steel
Kinetics MIM 316 Stainless Steel (Premium Grade)

MQM241B / 13790

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.