MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BP Amoco Innovene L57N-00 Injection Grade Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Formerly BP Amoco Fortilene® PP RG7910. Belongs to the new generation of Solvay polypropylenes produced by gas phase polymerization. This medium impact nucleated copolymer is intended for injection molding of household goods, packaging articles, etc. This resin is Kosher certified. This material meets the FDA requirements of 21CFR 177.1520 and U.L. 94HB flammability rating.

Information provided by Solvay Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.895 g/cc0.0323 lb/in³ASTM D792
Melt Flow 55 g/10 min55 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ASTM D2240
Tensile Strength, Yield 26.2 MPa3800 psi2 in/min.; ASTM D638
Elongation at Yield 10 %10 %2 in/min.; ASTM D638
Flexural Modulus, 1% Secant 1242 MPa180100 psi0.05 in/min; ASTM D790
Izod Impact, Notched 0.590 J/cm1.11 ft-lb/inASTM D256
Gardner Impact 13.8 J
@Thickness 3.17 mm,
Temperature -20.0 °C
10.2 ft-lb
@Thickness 0.125 in,
Temperature -4.00 °F
Test method CLP 463DB-14-01, 8 lb dart
Impact Test 10.9 J
@Thickness 2.00 mm,
Temperature 0.000 °C
8.04 ft-lb
@Thickness 0.0787 in,
Temperature 32.0 °F
Instrumented dart impact (Dynatup) at 0°C. Energy at break, 20mm tup, 50lb, 1m impact on 2mm thick part. ISO 6603
 
Thermal PropertiesMetricEnglishComments
Melting Point 164 °C327 °FASTM 3418
Crystallization Temperature 130 °C266 °FASTM 3418
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BP Amoco Innovene R10F-00 Concentrate/Filled Uses Grade Polypropylene
BP Amoco Innovene H25A-00 Injection Molding Grade Polypropylene
BP Amoco Innovene 1088 Polypropylene Homopolymer

PSOLMQ / 68305

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.