MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) 52528 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: 52528 is a HDPE copolymer injection molding grade for thin walled applications requiring a good balance between high flowability and physical properties.

Application: caps, thin walled, injection molding grade.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D1505
Melt Flow 28 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 1380 MPaASTM D790
Izod Impact, Notched 21.0 J/mASTM D256/A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 120 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) 52518 High Density Polyethylene
Iran Petrochemical (PCC) 6040UA High Density Polyethylene
Iran Petrochemical (PCC) I4 HD 7255 High Density Polyethylene
Iran Petrochemical (PCC) 5218EA High Density Polyethylene
Iran Petrochemical (PCC) 7000F High Density Polyethylene

PIPC215 / 149677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.